Selection and smelting of Tin Bronze raw materials

Dec 04, 2020

     Tin-phosphorus bronze generally uses low-frequency cored induction heating furnace for smelting and thermal insulation. During the whole process of early smelting and forging,Tin Bronze the maintenance of the solution should be improved. Generally choose dry wood charcoal or grain bran to cover. The smelting temperature of tin phosphor bronze is about 1180~1250℃,Tin Bronze and the forging temperature is 1140~1180℃.

    Using horizontal continuous casting, the surface of the QSn6.5-0.1 tin-phosphorus bronze strip structure is fine equiaxed crystals,Tin Bronze and the inner layer is columnar crystals. In the past,Tin Bronze the "pull-stop" procedure was used. When there is a "stop" in the rolling steel,Tin Bronze the primary crystal region is generated and the metal material is smelted in the extra crystal region that appears on the inner wall of the continuous casting mold. There is an interface zone between each other,Tin Bronze and it is easy to produce hydroxides,Tin Bronze doping, and Sn-rich low-melting point components.

    The appearance is mainly represented by the horizontal crystal texture on the surface of the cast slab. This kind of crystal texture is the embodiment of the whole forging process and the quality of the casting billet. Excellent crystal texture does not do much harm to the characteristics of the cast slab;Tin Bronze while the poor forging texture surface layer forging shrinkage is very large,Tin Bronze and it is very easy to cause edge regular cracking when cold rolled afterwards; when the "crystal texture" is significantly different , 

    Which shows that the actual cooling effect of continuous casting mold is uneven,Tin Bronze and it will also produce more serious forging shrinkage. Usually,Tin Bronze gray-white dissolved substances appear on the side with advanced texture, resulting in cracks.


Send Inquiry