1. Strictly add the materials in a reasonable order. For example, before adding aluminum or silicon components, the copper liquid needs to be deoxidized first, or added after adding the alloy components that have the deoxidizing effect and are easier to remove oxides from the copper liquid, such as zinc Manganese etc.
2. Carry out refining treatment.
3. Deoxidize at a higher superheat temperature and stir carefully.
4. When casting, the liquid flow should be short. Use bottom injection, filter screen and open gate to avoid secondary oxidation.
5. Limit the amount of recycled materials and strictly implement the smelting process.