1. The heating temperature of 350 ± 10℃ is more suitable. If the heating temperature of the tin bronze plate is too high, the workpiece will be seriously oxidized; if the temperature is too low, the strength and elasticity of the workpiece will be higher and the toughness will be obviously insufficient, so it is not suitable for forming. Due to the large amount of furnace installed, in order to allow it to pass through heat and obtain a certain degree of strength and toughness, to facilitate the subsequent bending processing, each furnace workpiece needs to be kept warm for about 2 hours after it reaches temperature, and then it can be air-cooled or left. Cool slowly in a tempered barrel.
2. Due to the limitation of conditions, two methods can be used to identify the processed workpiece simply. One is to observe the color of the workpiece, that is, the color of the processed workpiece changes from the original brass color to blue and black; the other is to treat the workpiece. The finished workpiece is directly bent by hand to judge. When bending, if you feel that the workpiece can be bent while having a certain strength and elasticity, it means that the annealing effect is good and it is suitable for forming. On the contrary, the processed workpiece has high strength and elasticity, and it is not easy to bend by hand, indicating that the annealing treatment effect is not good, and it needs to be re-annealed.
3. Adopt equipment and furnace installation method. In order to achieve the purpose of uniform temperature and anti-oxidation, the tin bronze material workpiece is generally not suitable for processing in a box furnace without a stirring fan. For example, under the condition of the same furnace load, the workpieces are compared in a box furnace without a stirring fan and a pit tempering furnace with a stirring fan. The treatment results of the tin bronze plate are very different under the same annealing process conditions of heating at 350 ± 10 ℃, holding for 2 hours and then air cooling.
www.cn-czpufa.com